US20070186798A1 - Tamping blade for a railroad tamping machine - Google Patents
Tamping blade for a railroad tamping machine Download PDFInfo
- Publication number
- US20070186798A1 US20070186798A1 US11/356,400 US35640006A US2007186798A1 US 20070186798 A1 US20070186798 A1 US 20070186798A1 US 35640006 A US35640006 A US 35640006A US 2007186798 A1 US2007186798 A1 US 2007186798A1
- Authority
- US
- United States
- Prior art keywords
- wear
- tamping
- railroad
- blade
- pad
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A tamping blade for a railroad-tamping machine to tamp ballast on a railway line. The tamping blade includes a pad that attaches to a shank of a railroad-tamping machine and is made of hardened steel. A wear-resistant coating covers and protects the surfaces used to tamp the ballast. Wear-resistant inserts are fixed in a leading face of the pad to absorb a large portion of the impact and improve the efficiency of the tamping process. The wear-resistant inserts are positioned to reduce the formation of a wear pattern during use. The method allows for production of a hardened steel pad with a wear-resistant coating and wear-resistant inserts.
Description
- The present invention relates to a tamping blade for a railroad-tamping machine, and more particularly to a tamping blade having an improved structure to resist wear and a method for producing the tamping blade.
- During use of railroads, ballast supporting the railroads shifts away from the railroad ties. Railroad tamping machines maintain ballast to provide correct alignment and elevation of rails. These tamping machines employ tamping tools that push multiple vibrating blades into the ballast and then towards the rail to compact the ballast supporting the rail. This provides a firm foundation for the rail to support the load of the trains passing over it. This procedure subjects the tamping blade to extremely harsh conditions, as typical ballast includes materials such as rock, wooden cinders, concrete, slag and taconite. Because the ballast also becomes compacted, the tamping blade must break up the ballast in order to repair the ballast. The abrasive nature of the ballast causes tamping blades to wear quickly, necessitating repair or replacement. Each railroad-tamping machine can employ from sixteen to thirty-two tools. Thus, wear and replacement leads to significant expense both in time lost and the cost of replacement blades.
- Many attempts have been made to increase the life of tamping blades by employing wear-resistant materials such as tungsten carbide. For example, U.S. Patent Application No. 2005/0109235 discloses a tamping tool that has a wear-resistant tip inserted into a groove in the end of its blade. Wear-resistant tiles are fixed on the portions of the blade to further protect the blade. Similarly, U.S. Pat. No. 5,261,763 describes a tamping tool having a paddle of carbon steel construction with wear-resistant material brazed to the front, exposed face of the paddle.
- Current tamping blades employing wear-resistant materials are generally made using a soft metal pad. As long as the pad is not exposed to abrasion, and is protected by wear-resistant material, the pads will be fine. But when the wear-resistant material chips off, or the metal pad is otherwise exposed, the soft metal quickly wears away and the tamping blade must be replaced. There is therefore a need for a tamping blade that is less affected by chipping.
- During use, the tamping blade must often break up the ballast. Current tamping blades employ a blunt leading face. The blunt leading face tends to incur impact along the entire length of the leading face and is inefficient for breaking up ballast. Concentrating the impact in a smaller area facilitates breaking up ballast. The stress at the point of impact is greater for a non-blunt blade. There is therefore a need for a tamping blade having a non-blunt leading face capable of withstanding the stress and wear occurring at the point of impact.
- Hardening the metal pad also improves resistance to wear by abrasion. It is therefore desirable to combine wear-resistant material with a hardened metal pad. However, application of wear-resistant material by brazing or welding causes softening of hardened metal, rendering a heat treatment process useless. Using a heat treatment processes after application of a wear-resistant material, such as carbide, would cause the joining material, such as a brazing silver solder to melt off. There is therefore a need for a tamping blade that combines a heat-treated pad with a wear-resistant material and a process to manufacture a tamping blade that combines a heat-treated pad with a wear-resistant material.
- The present invention therefore discloses a tamping blade for a railroad-tamping machine to tamp ballast on a railway line. The tamping blade includes a pad that attaches to a shank of a railroad-tamping machine and is made of hardened steel. A wear-resistant coating covers and protects the surfaces used to tamp the ballast. Wear-resistant inserts are fixed in a leading face of the pad and absorb the greatest impact, as well as increase the efficiency of the tamping process. The wear-resistant inserts are positioned to reduce the formation of a wear pattern during use. The method for producing the tamping blade allows for use of a hardened steel pad with a wear-resistant coating and wear-resistant inserts.
- These and further objects and advantages of the present invention will become clearer in light of the following detailed description of an illustrative embodiment of this invention described in connection with the drawings.
- The illustrative embodiment may best be described by reference to the accompanying drawings where:
-
FIG. 1A shows a perspective view of one embodiment of the tamping blade of the invention. -
FIG. 1B shows a top view of one embodiment of the leading face of the tamping blade of the invention. -
FIG. 2A shows a side view of a wear-resistant insert of the invention. -
FIG. 2B shows a side view of a second embodiment of a wear-resistant insert of the invention. -
FIG. 2C shows a side view of a third embodiment of a wear-resistant insert of the invention. -
FIG. 3 shows a flow diagram of a method for producing the tamping blade of the invention. - All figures are drawn for ease of explanation of the basic teachings of the present invention only; the extensions of the figures with respect to number, position, relationship, and dimensions of the parts to form the preferred embodiment will be explained or will be within the skill of the art after the following description has been read and understood. Further, the exact dimensions and dimensional proportions to conform to specific measurements will likewise be within the skill of the art after the following description has been read and understood. Values provided are representative and are utilized to facilitate the description of the preferred embodiment.
- Where used in the various figures of the drawings, the same numerals designate the same or similar parts. Furthermore, when the terms “upper,” “lower,” “side,” “end,”“bottom,” “first,” “second,” “laterally,” “longitudinally,” “row,” “column,” “array,” and similar terms are used herein, it should be understood that these terms have reference only to the structure shown in the drawings as it would appear to a person viewing the drawings and are utilized only to facilitate describing the illustrative embodiment.
- Refer now to
FIG. 1A , which shows a perspective view of one embodiment of thetamping blade 10 of the invention. Thetamping blade 10 includes apad 12. Thepad 12 includes anattachment location 14 where thepad 12 can be attached to a shank of a railroad-tamping machine by welding or other known methods. The welding process should not exceed 350 degrees F. in order to avoid softening thepad 12. The welding process can be done over a longer period of time in order to avoid too much heat being applied to thepad 12. Thepad 12 further includes a leadingface 16 suitable for breaking up ballast and moving and compacting ballast to properly support a rail. - In order to withstand the harsh environment involved in tamping ballast, the
pad 12 is preferably hardened. In the preferred embodiment, thepad 12 comprises a four inch (4″) by four and one-half inch (4½″) by three-fourths inch (¾″) 4140 steel pad having a hardness rating of around fifty-five (55) on a Rockwell C scale. As those skilled in the art will recognize, other conformations of thepad 12 are possible and lie within the spirit and scope of the invention. - To further protect the
surfaces 36 coming into contact with the ballast, thepad 12 includes a wear-resistant coating 18. In the preferred embodiment, the wear-resistant coating 18 covers the portions of the bordering faces 20, 22, 24, 26 adjacent to the leadingface 16. In this example embodiment, the wear-resistant coating 18 is a continuous coating made of tungsten carbide covering at least one inch (1″) from the edge adjoining the leadingface 16 on each of the bordering faces 20, 22, 24, 26. In this example embodiment, thecoating 18 has an average thickness of at least one-eighth of an inch (⅛″). In an alternate embodiment, the wear-resistant coating 18 also covers the leadingface 16. - The
tamping blade 10 further includes a plurality of wear-resistant inserts 28. In the preferred embodiment, the wear-resistant inserts may be made from tungsten carbide or other hardened material. Priorart tamping blades 10 commonly employ a blunt leading edge. Thetamping blade 10 of the invention includes a plurality ofhardened inserts 28 having asecured end 30 fixed within the leadingface 16 and having a protrudingend 32 extending from the leadingface 16. - As shown in
FIG. 1B , in the preferred embodiment thetamping blade 10 includes a plurality of holes machined into the leadingface 16. In one example embodiment, the plurality ofholes 34 are machined to be three-quarters of an inch deep (¾″). The hardened inserts 28 are one inch in length, cylindrical in shape and have asecured end 30 inserted into the plurality ofholes 34, resulting in theprotruding end 32 of thehardened insert 28 extending one-quarter of an inch (¼″) from thesurface 36 of the leadingface 16. The plurality of holes can be machined to arrange thehardened inserts 28 in a “jogged” pattern. The “jogged” pattern can be used to reduce formation of wear patterns on thetamping blade 10 during use. In this preferred embodiment, ten holes are machined into the leadingface 16, with each hole spaced one-eighth of an inch (⅛″) from the subsequent hole and having an offset of three-sixteenths of an inch ( 3/16″) from acenterline 38. Alternatively, the plurality ofholes 34 can be machined to arrange thehardened inserts 28 in a straight line. Those skilled in the art will recognize that other spacings and patterns can be employed and lie within the spirit and scope of the invention. - In the preferred embodiment, the plurality of
holes 34 have a dimension less than the wear-resistant inserts 28. This allows attachment of the wearresistant inserts 28 without welding or use of other material. A hammer or arbor press can be used to press fit the wear-resistant inserts 28 within thetamping blade 10. In this example embodiment, the plurality ofholes 34 have a diameter 0.002 inches less than the wearresistant inserts 28. - The protruding
end 32 of thehardened inserts 28 allows for more efficient and less-wearing breaking up of ballast. The hardened inserts 28 concentrate the force of thetamping blade 10 into a smaller area, allowing for easier breaking up of ballast, thereby requiring less energy. During the horizontal vibration of thetamping blade 10 during the tamping process, the protrudingend 32 of thehardened inserts 28 provides a raking effect to shift the ballast into the desiredlocation 14. In the preferred embodiment, thehardened inserts 28 comprise tungsten carbide or other wear-resistant material, such as hardened D2 steel. As those skilled in the art will recognize, other conformations and dimensions of thehardened inserts 28 on thetamping blade 10 can be employed without departing from the spirit and scope of the invention. - The protruding
end 32 of thehardened insert 28 may be shaped to best suit a desired application as shown inFIGS. 2A, 2B and 2C. In one preferred embodiment, the protrudingend 32 has an ovoid shape, as shown inFIG. 2A . In a second preferred embodiment, the protrudingend 32 has a conical shape, as shown inFIG. 2B . In a third preferred embodiment, the protrudingend 32 has a chisel shape, as shown inFIG. 2C . In one example embodiment, an ovoid shape can be used to break up granite ballast. A conical shape may be employed in hard limestone. A chisel shape can be used in sands and soft limestones. -
FIG. 3 shows a flow diagram of a method for producing thetamping blade 10 of the invention. Prior art tamping blades are hampered by the use of softer metal to provide thebase pad 12. Because the process of soldering wear-resistant material to abase pad 12 would cause softening of the metal used to form the base pad, there is little value to hardening thebase pad 12 prior to attachment of a wear-resistant material. After attachment of the wear-resistant material, thepad 12 cannot be subjected to the high heat required for heat treatment, often as high as 1550 degrees Fahrenheit. This heat would result in melting the silver solder or glue used to attach the wear-resistant material. - In contrast, the method for producing a
tamping blade 10 of the present invention allows for use of a wear-resistant material with ahardened pad 12. The method begins with forming apad 12 instep 100. In the preferred embodiment, thepad 12 is formed as a four-inch (4″) by four-and-one-half inch (4½″) by three-fourths inch (¾″) 4140 steel pad. - Next, the method applies a wear-
resistant coating 18 on the portions of bordering faces 20, 22, 24, 26 adjacent to the leadingface 16 instep 110. In this example embodiment, the wear-resistant coating 18 is a continuous coating made of tungsten carbide covering at least one inch (1″) from the edge adjoining the leadingface 16 to the bordering faces 20, 22, 24, 26. In an alternate embodiment, the wear-resistant coating may also cover a portion or all of the leadingface 16 in addition to the bordering faces 20, 22, 24, 26. - After application of the wear-
resistant coating 18, the method proceeds with machining a plurality ofholes 34 in the leading face instep 120. The plurality ofholes 34 can be machined in various patterns to improve the wear resistance of thetamping blade 10. In one example embodiment, a “jogged” pattern as shown inFIG. 1 improves resistance against formation of a wear pattern compared with a simple straight-line pattern. In the preferred embodiment, the plurality ofholes 34 are machined to have a diameter smaller than the diameter of wear-resistant inserts 28 to be inserted into the leadingface 16. - The pad is then heat-treated in
step 130 to a hardness rating of at least forty on a Rockwell C scale, compared to the usual hardness rating of eighteen of typical pads. In the preferred embodiment, the pad has a hardness rating between forty and sixty. In this example embodiment, a hardness rating of fifty-five can be attained by a typical heat treatment process of heating the pad to a temperature approximately 1500 degrees F., controlled cooling, and tempering by reheating. - The method for producing a
tamping blade 10 then provides for attachment of a wear-resistant insert 28 in each of the plurality ofholes 34 in the leadingface 16 instep 140. An arbor press can be used to press fit the wear-resistant inserts 28 into the plurality ofholes 34. Alternatively, a hammer can be used to press fit the wear-resistant 28 inserts into the plurality ofholes 34. In the preferred embodiment, the wear-resistant insert 28 has aprotruding end 32 that is shaped according to an intended use. - As the invention disclosed herein may be embodied in other specific forms without departing from the spirit or general characteristics thereof, some of which forms have been indicated, the embodiments described herein are to be considered in all respects illustrative and not restrictive. The scope of the invention is to be indicated by the appended claims, rather than by the foregoing description, and all changes which come within the meaning and range of equivalency of the claims are intended to be embraced therein.
Claims (20)
1. A tamping blade for a railroad tamping machine to tamp ballast on a railway line, the tamping blade comprising:
a pad having an attachment location and a leading face, with the attachment location providing for attachment to a shank of the railroad tamping machine and the leading face having a plurality of holes, with each of the plurality of holes spaced from one another; and
a plurality of wear-resistant inserts, with each of the plurality of wear-resistant inserts having a secured end fixed within a corresponding one of the plurality of holes and a protruding end extending from the leading face of the pad.
2. The tamping blade for a railroad-tamping machine of claim 1 with the plurality of wear-resistant inserts further comprising tungsten carbide inserts.
3. The tamping blade for a railroad-tamping machine of claim 1 with the plurality of wear-resistant inserts further comprising hardened D2 steel inserts.
4. The tamping blade for a railroad-tamping machine of claim 1 with the plurality of wear-resistant inserts having a press-fit attachment to the pad.
5. The tamping blade for a railroad-tamping machine of claim 1 with the plurality of holes spaced from one another in a jogged pattern to resist formation of a wear pattern during use.
6. The tamping blade for a railroad-tamping machine of claim 1 with the tamping blade further comprising a wear-resistant coating.
7. The tamping blade for a railroad tamping machine of claim 6 further comprising side faces having an edge adjoining the leading face, with the wear-resistant coating comprising a spray coating of tungsten carbide on each side face extending at least one inch from the edge adjoining the leading face.
8. The tamping blade for a railroad tamping machine of claim 6 further comprising side faces having an edge adjoining the leading face, with the wear-resistant coating comprising a spray coating of tungsten carbide on at least a portion of the leading face and on each side face extending at least one inch from the edge adjoining the leading face.
9. The tamping blade for a railroad tamping machine of claim 1 with the pad further comprising a four inch (4″) by four and one-half inch (4½″) by three-fourths inch (¾″) 4140 steel pad having a hardness rating of at least forty (40) on a Rockwell C scale.
10. The tamping blade for a railroad-tamping machine of claim 1 with the protruding end of the wear-resistant inserts having an ovoid shape.
11. The tamping blade for a railroad-tamping machine of claim 1 with the protruding end of the wear-resistant inserts having a conical shape.
12. The tamping blade for a railroad-tamping machine of claim 1 with the protruding end of the wear-resistant inserts having a chisel shape.
13. A tamping blade for a railroad tamping machine to tamp ballast on a railway line, the tamping blade comprising:
a pad having an attachment location, a leading face and side faces having an edge adjoining the leading face, the pad further having a hardness of at least forty (40) on a Rockwell C scale; and
a wear-resistant coating on each side face extending at least one inch from the edge adjoining the leading face.
14. The tamping blade for a railroad-tamping machine of claim 13 with the leading face of the pad further comprising:
a plurality of holes, with each of the plurality of holes spaced from one another; and
a plurality of wear-resistant inserts, with each of the plurality of wear-resistant inserts having a secured end fixed within a corresponding one of the plurality of holes and a protruding end extending from the leading face of the pad.
15. The tamping blade for a railroad-tamping machine of claim 13 with the wear-resistant coating further comprising tungsten carbide.
16. A method for producing a tamping blade for a railroad tamping machine, the method comprising:
providing a pad having a leading face and side faces adjacent to the leading face;
applying a wear-resistant coating to the pad; and
heat-treating the pad to a hardness rating of at least forty (40) on a Rockwell C scale.
17. The method for producing a tamping blade of claim 16 further comprising:
machining a plurality of holes in the leading face; and
attaching a plurality of wear-resistant inserts, each of the wear-resistant inserts having a secured end and a protruding end, and with a respective one of the plurality of wear-resistant inserts attached by having a secured end press-fit within each of the plurality of holes.
18. The method for producing a tamping blade of claim 17 with machining a plurality of holes in the leading face further comprising machining the plurality of holes to have a diameter smaller than the diameter of the wear-resistant inserts, and with attaching a plurality of wear-resistant inserts further comprising press-fitting the wear resistant inserts into the plurality of holes.
19. The method for producing a tamping blade of claim 16 with attaching a plurality of wear-resistant inserts further comprising selecting a plurality of wear-resistant inserts having a protruding end having a shape suitable to a predetermined application.
20. The method for producing a tamping blade of claim 16 with applying a wear-resistant coating to the pad further comprising fusing tungsten carbide on the side faces using a thermal spray powder procedure.