US20070163876A1 - Electrowetting cell and method of manufacturing an electrowetting cell - Google Patents
Electrowetting cell and method of manufacturing an electrowetting cell Download PDFInfo
- Publication number
- US20070163876A1 US20070163876A1 US11/568,734 US56873405A US2007163876A1 US 20070163876 A1 US20070163876 A1 US 20070163876A1 US 56873405 A US56873405 A US 56873405A US 2007163876 A1 US2007163876 A1 US 2007163876A1
- Authority
- US
- United States
- Prior art keywords
- wall
- substrate
- end section
- cell
- electrowetting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
The electrowetting cell (15) comprises an outer wall (90) and an inner wall (80), said outer wall (90) being provided with extensions (85,86) extending on opposing sides of the inner wall (80). The cell (15) is further provided with a membrane (45) for volume expansion and is sealed through an electroplated layer (95).
Description
- The invention relates to an electrowetting cell comprising a body section provided with a substrate and at least one side wall, which substrate and side wall jointly define a cavity containing electrowetting fluids and further comprising at least one end section secured to the body section.
- The invention also relates to a method of manufacturing an electrowetting cell comprising a body section provided with a substrate and a side wall, which substrate and side wall jointly define a cavity containing a first and a second electrowetting fluid.
- Electrowetting cells are cells in which light is refracted by a meniscus between two immiscible fluids. One of the two fluids is electrically insulating and the other is electrically conducting. The shape of the meniscus is variable under the influence of a voltage between two electrodes, one of which is connected to the electrically conducting fluid and the other to a surface of the body. Such cells are known and can for instance be applied as lenses or displays. In the case of the application of a cell, there is a light-path through the body section.
- Such an electrowetting cell is for instance known from WO-A 03/069380. This patent application discloses a lens in which an inner surface of the at least one side wall is covered by a hydrophobic fluid contact layer. When no voltage is applied, the wettability of the fluid contact layer with respect to the electrically insulating fluid differs from the wettability of the fluid contact layer with respect to the electrically conducting fluid. Under influence of the applied voltage a change of the wettability occurs. This leads to a change of a contact angle of the meniscus at a line of contact between the fluid contact layer and the fluids, whereby the shape of the meniscus is adjusted. Hence, the shape of the meniscus is dependent on the applied voltage.
- As the electrowetting cell has optical properties and includes fluids, it is of primary importance for an adequate operation that a complete filling of the cell is achieved and that no fluid can leak out of the cell after closing the cell. The cell disclosed in the prior art does not give any solution as to how to achieve such a complete filling and prevent fluid leakage.
- It is therefore a first object of the invention to provide an electrowetting cell of the kind mentioned in the opening paragraph, which can be completely filled and is protected against fluid leakage after closing of the cell.
- It is a second object to provide a method of the kind mentioned in the opening paragraph, with which the complete filling can be achieved in an industrially viable manner.
- The first object is achieved in that the at least one side wall of the body section comprises an inner wall and an outer wall, a portion of which end section is part of the inner wall, thus securing the end section and the body section, and which outer wall is provided with extensions extending on a first side and a second side of the inner wall opposed to the first side.
- The second object is achieved in a cell with an inner and an outer wall, said outer wall having a first and second extension extending on opposite sides of the inner wall; which method comprises the steps of:
- providing an outer wall and a substrate, resulting in the cavity;
- filling the cavity with the first and the second electrowetting fluid;
- providing the end section in the cavity such that it is immersed in at least one of the fluids at a desired distance to the substrate, portions of the substrate and the end section and optionally an intermediate spacer forming the inner wall; and
- securing the end section to the body section in that the first extension of the outer wall is positioned on top of the end section.
- The solution of the present invention is a double-walled cell. The outer wall provides stability and adequate sealing, whereas the inner wall is built up from the constituent elements that are assembled consecutively. Due to the consecutive assembly and the double wall, the electrowetting fluids can be provided before the end section. As a result, the end section can be immersed in the fluid, in practice the fluid with the lowest density. Some fluid will flow to above the end section, but is nevertheless kept within the outer wall. The immersion leads to the required complete filling. An adequate sealing is then arrived at, in that the outer wall is present on the opposite sides of the inner wall. The outer wall of the package will then comprise only two major materials, which can be attached to each other in a good manner. A suitable combination is metal and glass.
- The substrate could be part of the outer wall, but is preferably a separate part of which an portion is part of the inner wall. A spacer may be present between the portions of the substrate and the end section. This is suitable but not necessary. The advantage of such spacer is that it can be provided with any desired surface coating, such as the above mentioned fluid contact layer. Advantageously, the spacer is provided with a gap on its bottom side. This allows a reduction of the height of the cell.
- Several embodiments can be envisaged for the first extension that is provided on top of the end section. It may for instance be a flexible extension of the outer wall. It may alternatively be a metal layer that is positioned through a deposition technique, probably with the help of a tool exerting pressure.
- In a preferred embodiment, the first extension is a clamping body that is assembled on top of the end section as a separate component and—simultaneously or consecutively—connected to the outer wall. This allows an efficient assembly method. Reliable connection can be realized in both mechanical and chemical means, such as locking features, additional clamps, adhesive layers and sealing layers. Advantageously, use is made of a joining and protective layer that is grown on said surfaces. The grown layer is chemically bonded to the surfaces. It has the same coefficient of thermal expansion and it is not sensitive to inelastic and irreversible expansion under the influence of temperature. The grown layer can be grown to a desired thickness, therewith smoothening out gaps and height differences. Moreover, such a grown layer is quite inert, particularly if provided with an oxide, which may be a native oxide. Finally, the grown layer is not sensitive to attack by any of the electrowetting fluids and does not have an open or porous structure that would allow diffusion of molecules. With such a sealing, particularly together with a substrate and end section of glass, the resulting cell is closed hermetically.
- A particularly suitable technique hereto is electroplating. This technique has the advantage that it can be applied at bulk level, by immersing the complete cell into a bath. Such an immersion of the complete cell moreover has the advantage that the grown layer extends on the complete outer wall and on both extensions on either side of the inner wall. Herewith the clamping character of the outer wall is strengthened.
- In a further embodiment, a first and a second electrode which are in contact with at least one of the electrowetting fluids are defined on opposed sides of the cavity in the substrate and at the end section. At least two electrodes are needed in the electrowetting cell so as to apply the voltage needed to set the shape of the meniscus. Such electrodes can be applied at the inner walls, on opposite sides of the meniscus. In this embodiment however, the electrodes are present at the end section and on the substrate. This actually allows the use of a metal encapsulation without an insulated connection for one of the electrodes.
- Preferably, the substrate is provided with an aperture, at an end of which said electrode is present. The electrode may be present both on a surface of the substrate facing the meniscus and on an opposite surface facing away from the meniscus. The latter modification is preferred, as there is no need to fill said aperture with metal herein: the fluid fills the aperture. Moreover, the manufacture of this electrode can be integrated with the provision of metal strips that are used for the attachment of the outer wall to the substrate, and hence provide an adequate sealing.
- It is preferred that the package is provided with a volume expansion member. Such an expansion member is for instance known from JP-A 2002/162506. This known package comprises a specific chamber that is present adjacent to the substrate, and is separated from the cell with a flexible cover. On increase of the pressure in the cell, the flexible cover may be deformed or even be stretched out, so as to form a curved surface extending into the said chamber. The invention offers the possibility to locate such a chamber between the inner wall and the outer wall.
- A more preferable embodiment of the volume expansion member is a flexible membrane that is part of the end section. In this manner, a larger part of the end section—that is: the part that is present in the light path—is moved. Hence, a substantial volume increase can be compensated. The flexible membrane is particularly ring-shaped. The end section is thus divided into an outer edge, a membrane and an inner portion. The standard position of the end section need not to be planar herein. As will be explained with respect to the figures, it is particularly such that the outer edge is pushed downwards under the pressure of the clamping body. This moreover results in a pressurized package. Although not preferred, it is not excluded that the outer edge portion of the end section comprises another material than the inner portion.
- The membrane is more preferably made of metal. Such a material withstands the fluids effectively. It has the additional advantage that the membrane can be used as one of the electrodes of the cell. If the connection between clamping body and outer wall is provided by electroplating or the like, the membrane will be provided with a metal layer too. A suitable thickness of the membrane layer that has sufficient stability on the one hand and sufficient flexibility on the other hand, is in the order of 5-30 microns, and more preferably between 15 and 25 microns. This is also dependent on the material of the membrane. In order to limit the thickness of the membrane, it may be provided with an insulating coating.
- The substrate and the end section are preferably glass plates. Glass is inert against the electrowetting fluids. It can be treated with techniques such as powder blasting, and metal layers can be attached to it. If desired, one or both glass plates may be provided with coatings and surface layers, including IR-coatings, UV-absorption coatings, antireflection coatings, but also lenses. Such lenses can be made of surface layers with the replica technique. Alignment features may be included in such replica made surface layers. This allows a proper alignment of the cell with further lenses on the bottom and the top side.
- If the cell of the invention is used as a lens, it is suitably assembled with further lenses to obtain a desired path. It is not excluded that two electrowetting lenses are part of the assembly; in fact this provides zoom properties. An alternative embodiment is however a stacked electrowetting lens. This stacked electrowetting lens can be suitably made with the method of the invention.
- In a first embodiment of stacked cell manufacture, the substrate is present located in the middle of the stacked cell construction. A first assembly and filling then takes place on the one side of the substrate, and a second assembly and filling takes place on the opposed second side after finalizing the assembly and filling on the first side. Preferably both opposite end sections are provided with a flexible membrane for compensation of volume expansion. The outer wall is provided in this construction with an extension to support the substrate halfway the stacked cell.
- In a second embodiment of the stacked cell manufacture, the two cells are provided within the outer wall one after the other. The end section of the first cell may be the substrate of the second cell, but that is not necessary. Most simply, a spacer is provided instead of the clamping body. On this spacer, which may well be connected to the outer wall by electroplating, a further substrate and the further elements of the second cell are provided consecutively. Such a construction moreover allows the electrodes to be located in the substrates and the end sections not needing mutual coupling.
- Instead of stacking of several electrowetting cells, the outer wall may be applied for stacking of one electrowetting cell and further optical and/or non-optical elements. In addition to separate lenses and filters, it is envisaged that an image sensor is assembled in this manner, separated from the electrowetting lens at a desired distance with any spacer or the like. Such an integration is most effectively carried out with an image sensor in which the bond pads are located on a surface opposite the optically active surface. Alternatively, the image sensor can be assembled on top of an interposer substrate, which is provided with through-holes so as to bring the contacts to a side opposite the optically active surface. The use of interposer substrates is known per se in the art of semiconductor packaging.
- It is an advantage of the method of the invention that it can be carried out at a wafer-level or a bulk level. The outer wall may be part of a plate, such as a printed circuit board with apertures. It can be separated into individual packages only after the filling and encapsulating steps. However, even if the manufacture of the cells is carried out individually, the electroplating steps can occur in a bath, allowing the simultaneous electroplating of a plurality of devices.
- The invention is further related to a manufacturing method and a cell of the kind mentioned in the opening paragraph, in which a hermetic sealing is provided. This is achieved in that the end section is attached to the body section with a metal layer that is applied on a surface of both the end section and the joint section. As is explained above, the application of a metal layer will lead to a hermetic sealing. A clamping is achieved if the metal layer, or the construction which the metal layer is part of extends on both sides of the cell. A preferred application method is electroplating, but other methods such as sol-gel deposition of metal, sputtering or chemical vapor deposition, or combinations of such deposition methods, are not excluded. The metal layer will suitably be attached to metal parts on the surface of the end section and on the surface of the body section.
- The cell may be used as a lens for use in a camera, in an optical recording apparatus or any other optical equipment. The cell may be assembled with further lenses, to obtain an optical path as needed, or even to obtain a zoom lens. Alternatively, the cell is used as a display, in which case only either the substrate or the end section needs to be optically transparent. The cell may be further used as a sensor.
- These and other aspects of the cell and the method of the invention will be further elucidated with reference to the figures, in which:
-
FIG. 1 shows a diagrammatical cross-sectional view of the cell of the invention, in which only the left part is depicted; -
FIGS. 2-7 show diagrammatic cross-sectional views of consecutive stages in the manufacture of the end section used in the cell; -
FIGS. 8-16 show diagrammatic cross-sectional views of consecutive stages in the method of manufacturing of the cell, in which Figures only the left part of the cell is depicted. -
FIG. 17 shows a diagrammatical cross-sectional view of a second embodiment of the cell of the invention. - The Figures are diagrammatic and not drawn to scale. The same reference numbers in different figures refer to like parts.
-
FIG. 1 shows an embodiment of anelectrowetting cell 15 according to the invention. In thisFIG. 1 only a partial cross-sectional view is shown, i.e. only the left part of thecell 15. Thecell 15 is however built up symmetrically, such that the non-shown right part is the mirror of the left part. The lens includes a fluid chamber, with afirst fluid 51 and asecond fluid 52, which are non-miscible and contact each other over ameniscus 14. Thefirst fluid 51 is in this example a silicone oil, an alkane or another suitable electrically insulating fluid. Thesecond fluid 52 is in this example water containing a salt solution or another suitable electrically conducting fluid. The sides of the chamber are provided with an electrically insulatinglayer 8 and afluid contact layer 10, for instance parylene. - According to this embodiment, the body section 17 comprises an
inner wall 80 and anouter wall 90, and—on thesecond side 112 of thecell 15—thesecond cover plate 6. Theinner wall 80 comprises an electrically insulatingmember 8 that is coated with afluid contact layer 10. Theinner wall 80 also comprises a portion of theend section 4. This end section (or first cover plate) 4 comprises a ring-shapedglass member 81 that is connected to an inner portion via an expandable joint 45. In a preferred embodiment, this ring-shapedglass member 81 and the inner portion of theend section 4 are manufactured from a single glass plate, as will be explained with reference to FIGS. 2 to 7. Theinner wall 80 further comprises theend 61 of thesecond cover plate 6. Thissecond cover plate 6 is provided with a throughhole 62, anelectrode 2, and ametallization 63. In an alternative embodiment, theplate 6 may be replaced by a construction similar or identical to that on thefirst side 111 of thecell 15, i.e. a ring-shaped glass member, an expandable joint and a cover plate. - These three sections of the
inner wall 80—the ring-shapedglass member 81, the—also ring-shaped—insulatingmember 8 and theend 61—are clamped between aprotrusion 85 of theouter wall 90 and a ring-shapedclosing member 86. The closingmember 86 is herein a piece of metal, but can be anything with an electrically conducting surface. Theouter wall 90 comprises an inner core of plastic orother material 92 that is provided with a metallizedsurface 91. This metallizedsurface 91 also bounds themetallization 63 of thesecond cover plate 6. In this manner, a mechanically stable connection is provided. - The
inner wall 80 and theouter wall 90 are attached to each other, as well as to the joint 45 and theend section 4, in that asealing layer 95 is present around it. Thesealing layer 95 can be made of a suitable material. Polymeric coating of rubber, epoxy or the like, as are known per se as protective coating may be used. It is however preferred that thesealing layer 95 comprises a metal. This allows the provision of a package that is hermetical and not prone to diffusion of air, water or fluid. A particularly preferred method for the provision of thismetal sealing layer 95 is electroplating. This method can be carried out on three-dimensional surfaces, e.g. in a bath. - FIGS. 2 to 7 show in schematic cross-sectional views consecutive steps in a method of manufacturing of the
substrate 200 with an integrated membrane 210, to be applied as expandable joint 46.FIG. 2 shows thesubstrate 200, with afirst surface 201 and an opposedsecond surface 202. Thesubstrate 200 is in this example a glass plate with a suitable thickness, for instance in the order of 0.1 mm. -
FIG. 3 shows thesubstrate 200, after aphotoresist 205 has been applied on bothsurfaces -
FIG. 4 shows thesubstrate 200 after patterning and developing thephotoresist 205. The patterning on thefirst side 201 results in anaperture 214. The patterning on thesecond side 202 has resulted in the fact that also thesurface 215 of thephotoresist 205 is given a three-dimensional structure. Thissurface 215 is in this example in the form of an undulating surface. This surface structure can be provided by forging or another manner of mechanical deformation. Alternatively, use is made of advanced photolithographical techniques. In an even further embodiment, use is made of a moulding technique to provide thephotoresist layer 205 in the desired shape. As will be understood, no specific photoresist material is needed in such a case. -
FIG. 5 shows thesubstrate 200 after amembrane layer 225 has been applied. The membrane layer comprises for instance a metal with some elasticity, although any other material is suitable, as long as it is compatible with thephotoresist layer 205. Many metals turn out to have sufficient flexibility if applied as a thin layer. Examples include gold, copper, nickel, aluminum, as well as suitable alloys thereof. A metal layer may be applied with a suitable deposition technique, such as sputtering, chemical vapor deposition and also wet-chemical techniques. In this example, themembrane layer 225 is shown to be patterned, but that is not necessary. -
FIG. 6 shows thesubstrate 200 after that it has been patterned through the patternedphotoresist 205 on thefirst side 201. In the case of aglass plate 200 the technique of power blasting can be applied advantageously, which, however, does not exclude any other technique such as etching. -
FIG. 7 shows thesubstrate 200 after thephotoresist 205 has been removed, and asubstrate 200 with an integrated membrane 220 results. As will be clear, thesubstrate 200 may extend in lateral directions. The membrane 220 may have any suitable shape. Particularly preferred is a ring shape. The substrate may contain a plurality of membranes, and be suitable for wafer-level processing in a further step, or be separated. Such a separation step could also be applied before the removal of thephotoresist 205. Although not shown here, it is not excluded that the substrate comprises further layers on its first orsecond side substrate 200, semiconductor elements such as diodes and transistors or trench capacitors may be defined herein. - FIGS. 8 to 16 show diagrammatical cross-sectional views of the method of manufacturing of the
electrowetting cell 15. Shown here is the manufacture of the embodiment ofFIG. 1 , but modifications and alternatives are possible within the scope of the present invention. -
FIG. 8 shows the first step in the assembly. Herein, aglass substrate 6 is provided in a ring-shapedmember 90. The ring-shapedmember 90 acts as an outer wall, and is provided with an electrically conducting surface. It is not necessary, though allowed, that the complete surface is electrically conducting. Themember 90 is provided with anextension 85, which is present on afirst side 112 of thesubstrate 6 and is in contact with aadhesion layer 63 of thesubstrate 6. Theadhesion layer 63 is here a metal, such as copper. Anelectrode 2 is present on the samefirst side 112 of thesubstrate 6. Thiselectrode 2 covers anaperture 62 in thesubstrate 6. Theaperture 62 may be filled with electrically conducting material, but that is not the case in this example. Theaperture 62 is—contrary to for instance theouter wall 90—not ring-shaped, but provided locally only. Instead of glass another material can be used. In case the cell is not a lens, there is no need for the substrate to be optically transparent. In order to keep thesubstrate 6 and the outer wall attached, for instance use is made of an adhesive layer. -
FIG. 9 shows the result after a second step in the assembly. Herein, thesubstrate 6 and theouter wall 90 are connected to each other with ametal layer 91. Thismetal layer 91 is suitably provided by electroplating in a bath. Themetal layer 91 extends around theouter wall 90, and is connected to theadhesion layer 63 of the substrate. The connection is present not only on thefirst side 112 of the substrate, but also on aside face 115. Shown here, but not in further figures is the fact that theelectrode 2 will be provided with an electroplated layer as well. The position of thiselectrode 2 is chosen such that no bridge is formed between the electrode and the outer wall. An insulating coating may be provided at theelectrode 2 in order to prevent the thickening thereof. -
FIG. 10 shows the result after an electrically conductingfluid 52 has been provided in theouter wall 90 and on thesecond side 113 of thesubstrate 6. In this example the fluid 52 is an aqueous salt solution. Alcohols and the like may be used as additional solvents. The fluid extends into theaperture 62, thereby making contact with theelectrode 2. Theelectrode 2 acts at the same time as a closure of the cell. -
FIG. 11 shows the result after the provision of the electrically insulatingfluid 51. This is an oil, for instance an alkane or a silicon oil. In view of its lower density, it is provided after the electrically conductingfluid 51. The shapes of the meniscus shown and the adhesion to thesecond side 113 of thesubstrate 6 are purely diagrammatical and do not necessarily correspond to any physical effect. -
FIG. 12 shows the result after the insertion of aspacer 8. This is in this case a ring-shaped electrically insulatingmember 8 that is provided with afluid contact layer 10 of parylene. Thespacer 8 has asurface 9 that may have a modified surface structure or layer for proper adhesion to the electroplatedlayer 91 of theouter wall 90. This surface structure or layer can be of any chemical kind, but also mechanical, such as a locking feature. Additionally, thespacer 8 is provided with agap 64. Thisgap 64 has as a first advantage that theelectrode 2 can be provided below thisspacer 8. Hence, theelectrode 2 is located outside the light path, which reduces the diameter of the cell. A second advantage of the gap is a modification of the angle of themeniscus 14 between the electrically conductingfluid 52 and the electrically insulatingfluid 51. As a result, the minimum thickness of the cell is reduced. Together with anouter edge 61 of the substrate the spacer forms part of the inner wall. -
FIG. 13 shows thecell 15 after a sixth manufacturing step. This step involves the assembly of theend section 4. Theend section 4 includes an inner portion, amembrane 45 and anouter portion 81. Apressure tool 70 is provided on afirst side 111 of theend section 4. Preferably, theend section 4 is provided with a layer of the electrically insulating fluid on itssecond side 114 before the actual assembly. This ensures that no air bubbles will be formed during the assembly. Theend section 4 is immersed in the fluid 51 during the assembly. As a result thereof, asurplus layer 55 of the fluid is formed on the first side of the end section. The electrically insulatingfluid 51 is able to flow from thesecond side 114 to thefirst side 111 of theend section 4, as a narrow channel is left between theouter portion 81 and theouter wall 90. -
FIG. 14 shows thecell 15 after theouter portion 81 of theend section 4 has been secured to the body section. This body section comprises in fact both thespacer 8 and theouter wall 90. This is carried out by insertion of a clampingbody 86. This body clamps and/or puts theouter portion 81 downwards to thespacer 8. As a result themembrane 45 is put in a slightly bent position. The clamping body has a surface that is in contact with the electroplatedsurface layer 91 of theouter wall 90. It is preferably provided with one or more locking features. If desired, it may be designed to extend into thechannel 89 between theouter portion 81 and theouter wall 90. In this operation, theinner wall 80 is formed, constituted by theadhesive layer 63, theouter portion 61 of thesubstrate 6, thespacer 8, theouter portion 81 of theend section 4 and the clampingbody 86. -
FIG. 15 shows thecell 15 after removal of thetool 70 and thesurplus 55 of the electrically insulatingfluid 51. The removing step is followed by a cleaning step, so that the surfaces of the clampingbody 86 and themembrane 45 are sufficiently clean for subsequent steps. -
FIG. 16 shows thecell 15 after the last important step in the manufacture. In this step, the connection between the clampingbody 86 and theouter wall 90 is strengthened by the provision of asealing layer 95. Thesealing layer 95 is preferably provided by electroplating in a suitable bath. Alternatively, it may be any other protective layer known per se in the art, such as an epoxy-based layer. Thesealing layer 95 extends in this example to themembrane 45 but this is not essential. Preferably, thesealing layer 95 is provided in a suitable thickness so as to fill any comers and provide a smoothened outer surface. Thesealing layer 95 extends in this example from thefirst side 111 of the end section to thefirst side 112 of the substrate. This is advantageous, in that it therewith has a clamping character as well, and unifies theouter wall 90 with itsextensions -
FIG. 17 shows a diagrammatical, cross-sectional view of a second embodiment of the cell of the invention. Not shown in this embodiment are any electroplated sealing layers that cover theextension 85 of theouter wall 80. In this embodiment, thecore 92 of the outer wall is a metallic tray, which inherently comprises theprotrusion 85. Thesecond cover plate 6 with the through-hole 62, thebody member 8 and thefirst cover plate 4 is herein assembled in the manner described with reference to FIGS. 8 to 16. Thebody member 8 will generally operate as one of the electrodes, and it is for instance connected to thetray 92, which acts as a contact. - The
first cover plate 4 is herein a continuous plate that is chosen to be sufficiently thin so as to be bendable under stress. In this example, use is made of a plate of glass. There is acavity 41 between thebody member 8 and thefirst cover plate 4. Under expansion of at least one of thefluids first cover plate 4 will bend so as to enlarge the volume in the cell. Under shrinkage of at least one of thefluids fluid 51 is preferably an oil and has a larger coefficient of thermal expansion than the aqueoussecond fluid 52, it is preferable for the bendablefirst cover plate 4 to be present on the side of the electrically insulatingfluid 51. - Although not shown here, very good results have been obtained with the electroplated sealing layer. It is not excluded that this electroplated sealing layer is also applicable in other configurations of fluid containing cells, and that not for all applications a cell with both an
inner wall 80 and anouter wall 90 and anextension extensions outer wall 80 extending on the first andsecond side extension 86.
Claims (16)
1. An electrowetting cell comprising a body section provided with a substrate and at least one side wall, which substrate and side wall jointly define a cavity containing electrowetting fluids and further comprising at least one end section secured to the body section, wherein the at least one side wall of the body section comprises an inner wall and an outer wall, a portion of which end section is part of the inner wall, thus securing the end section and the body section, and which outer wall is provided with extensions extending on a first side and a second side of the inner wall opposed to the first side.
2. An electrowetting cell as claimed in claim 1 , wherein the inner wall comprises a portion of the substrate.
3. An electrowetting cell as claimed in claim 2 , wherein the inner wall further comprises a spacer of an electrically insulating material between said portion of the substrate and said portion of the end section.
4. An electrowetting cell as claimed in claim 1 , wherein the extension of the outer wall extending on the first side of the inner wall is a clamping body that is attached to the outer wall.
5. An electrowetting cell as claimed in claim 4 , wherein the clamping body is attached to the outer wall by means of a metal layer that is grown on the extension and on the outer wall.
6. An electrowetting cell as claimed in claim 1 , wherein a first and a second electrode which are in contact with at least one of the electrowetting fluids are defined on opposed sides of the cavity in the substrate and at the end section.
7. An electrowetting cell as claimed in claim 6 , wherein the substrate is provided with an aperture, at an end of which said electrode is present.
8. An electrowetting cell as claimed in claim 1 , wherein the end section comprises a flexible membrane allowing for volume expansion of the closed cavity.
9. An electrowetting cell as claimed in claim 2 , wherein the extension on the second side of the inner wall is attached to the substrate through a metal layer that is grown on both sides.
10. An electrowetting cell comprising a body section provided with a substrate and at least one side wall, which substrate and side wall jointly define a cavity containing electrowetting fluids, and further comprising at least one end section secured to the body section, wherein the end section is attached to the body section with a metal layer that is applied on a surface of both the end section and the joint section.
11. A method of manufacturing an electrowetting cell comprising a body section provided with a substrate and a side wall having an inner wall and an outer wall, said outer wall being provided with a first and a second extension extending on opposed sides of the inner wall, which substrate and side wall jointly define a cavity containing a first and a second electrowetting fluid, which method comprises the steps of:
providing an outer wall and a substrate, resulting in the cavity;
filling the cavity with the first and the second electrowetting fluid;
providing the end section in the cavity such that it is immersed in at least one of the fluids at a desired distance to the substrate, portions of the substrate and the end section and optionally an intermediate spacer forming the inner wall;
securing the end section to the body section in that the first extension of the outer wall is positioned on top of the end section.
12. A method as claimed in claim 11 , wherein the extension is a separate clamping body that is connected to the outer wall only after having been positioned on the end section.
13. A method as claimed in claim 12 , wherein the clamping body and the outer wall are connected with a metal layer grown on their surfaces.
14. An image capturing device or an image sensor incorporating an electrowetting cell as claimed in claim 1 .
15. An optical scanning device comprising an electrowetting cell as claimed in claim 1 .
16. A display device incorporating an electrowetting cell as claimed in claim 1.